IPC_NEW_RELEASES Archives

1998

IPC_New_Releases@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jessica Carter <[log in to unmask]>
Reply To:
Jessica Carter <[log in to unmask]>
Date:
Mon, 5 Oct 1998 11:17:01 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (27 lines)
IPC-9504
Assembly Process Simulation for Evaluation of Non-IC Components (Preconditioning
Non-IC Components)

This document is another in a series and specifically addresses preconditioning of
non-IC components used in electronic assembly.  Do the components work with your
process?  That determination is the goal of these manufacturing process simulations;
to ensure that the components chosen meet expected reliability requirements after
exposure to factory processes.  Developed for users and manufacturers, the procedure
consists of a set of simulations, for non-IC component storage and use, wave and
reflow soldering (SMT and PTH parts), exposure to corrosive (water soluble) fluxes,
and exposure to often-used cleaning materials.  19 pages.  Released June 1998.

IPC Member:  $20                       Nonmember:  $40

################################################################
IPC_New_Releases E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE IPC_New_Releases <your full name>
To unsubscribe:   SIGNOFF IPC_New_Releases 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2