IPC-CF-148A (e)
Resin Coated Metal Foil for Printed Boards
This specification establishes the requirements for metal foils coated with a resin
or composite of resins on one side, which are to be used for the fabrication of
printed boards. Also included are a series of specification sheets, which outline
engineering and performance data for resin coated metal foil, indicating foil
material type and resin type. Released September 1998.
Member Nonmember
Single: $23 $46
Five-user: $75 $150
20-user: $150 $300
Site: $525 $1,050
Global: $1,050 $2,100
################################################################
IPC_New_Releases E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE IPC_New_Releases <your full name>
To unsubscribe: SIGNOFF IPC_New_Releases
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|