IPC-600-6012 Archives

January 2010

IPC-600-6012@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lionel Fullwood <[log in to unmask]>
Reply To:
(Combined Forum of D-33a and 7-31a Subcommittees)
Date:
Fri, 29 Jan 2010 11:33:22 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (13 lines)
Hi All:

Assuming that this is the only observation made, and from a coupon, I 
would be hesitant to pass it WITHOUT looking at several more sections. The 
fact that it occured in a small sample might suggest that the core itself 
was badly constructed.  Recognizing that Polyimide Boards tend to operate 
in harsher conditions than normal FR-4 material I feel it needs further 
review.

Lionel.
** Email Disclaimer **
This message and any attachments are confidential and are intended only for the use of the addressee. If you are not the intended recipient, you should not disseminate, distribute or copy this communication. If you have received this communication in error, please notify us immediately by return email and delete the original message. We use virus scanning software but exclude all liability for viruses or similar in any attachment. Thank you.