IPC-600-6012 Archives

August 2006

IPC-600-6012@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Susan Hott <[log in to unmask]>
Reply To:
(Combined Forum of D-33a and 7-31a Subcommittees)
Date:
Fri, 4 Aug 2006 10:02:00 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (37 lines)
Clarence
The other part of the paper trail is that the board drawing should have referenced IPC-6012.  In that document it states that the solder mask should meet all of the requirements in SM-840 plus a few others.  

Susan Hott
President
Robisan Laboratory, Inc
6502 E 21st Street
Indianapolis, IN 46219

317-353-6249 phone
317-917-2379 fax

www.robisan.com



-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]]On Behalf Of Knapp,
Clarence W.
Sent: Thursday, August 03, 2006 5:16 PM
To: [log in to unmask]
Subject: [IPC-600-6012] Inspection of Solder Resist


I just run into a problem between IPC-A-600 and IPC-A-610. In the IPC
600 Solder Resist cracking is not addressed with the waves and wrinkles
so it is not inspected for and generally ignored. However, IPC-A-610
states that crack of the resist is a rejection. The enclosed picture is
an example of the crack on bare board.