IPC-600-6012 Archives

February 2008

IPC-600-6012@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Korf, Dana" <[log in to unmask]>
Reply To:
(Combined Forum of D-33a and 7-31a Subcommittees)
Date:
Mon, 4 Feb 2008 15:11:43 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (83 lines)
We have a couple of customers using bare copper with press-fit
connectors.

Dana


Dana Korf
Dir. Product Engineering
(W) 408-964-4617
(C) 925-922-0548
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Mike Hill
Sent: Monday, February 04, 2008 2:46 PM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] Bare Copper as a Surface Finish

All,

I had a customer last month that wanted "bare copper" with nothing on
it.
It was a RF circuit that he wanted to keep the skin effect to a minimum.

Mike

-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]]On Behalf Of John Perry
Sent: Monday, February 04, 2008 3:53 PM
To: [log in to unmask]
Subject: [IPC-600-6012] Bare Copper as a Surface Finish


Colleagues,

 

Our IPC-6012B specification provides for bare copper as a final finish
in Table 3-2, Final Finish, Surface Plating and Coating Thickness
Requirements.

 

The task group is evaluating whether or not this should be removed from
Table 3-2 in the future IPC-6012 Revision C.  Among the concerns with
bare copper are instances of single-sided via protection that provides
for entrapment of chemistries that attack the bare copper in the hole
wall.

 

If there are those of you out there who use bare copper as a surface
finish, could you provide feedback to IPC as to how it is used in your
applications?

 

Thanks in advance,

 

John Perry

Technical Project Manager

IPC

3000 Lakeside Drive # 309S

Bannockburn, IL 60015

[log in to unmask]

1-847-597-2818 (P)

1-847-615-7105 (F)

1-847-615-7100 (Main)

 

CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use by the addressee(s) named herein and may contain legally privileged and/or confidential information. If you are not the intended recipient of this e-mail message, you are hereby notified that any dissemination, distribution or copying of this e-mail message, and any attachments thereto, is strictly prohibited.  If you have received this e-mail message in error, please immediately notify the sender and permanently delete the original and any copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS NOT INTENDED AS A SUBSTITUTE FOR A WRITING.  Notwithstanding the Uniform Electronic Transactions Act or the applicability of any other law of similar substance and effect, absent an express statement to the contrary hereinabove, this e-mail message its contents, and any attachments hereto are not intended to represent an offer or acceptance to enter into a contract and are not otherwise intended to bind the sender, Sanmina-SCI Corporation (or any of its subsidiaries), or any other person or entity.

ATOM RSS1 RSS2