John,
This looks like the type of crack that Phil Henault was lobbying
to get put into IPC-A-600. The crack is within a glass fiber bundle, not
at the "knuckle". We consider this to be a laminate defect.
Thanks,
Lance
From:
John Perry <[log in to unmask]>
To:
[log in to unmask]
Date:
01/28/2010 05:40 PM
Subject:
[IPC-600-6012] Bundle Crack in Microsection
Sent by:
IPC-600-6012 <[log in to unmask]>
Hi Everyone,
We've got a request for feedback on the anomaly in the attached .ppt file
which was detected in one bundle of glass in a coupon. This is in the
center of the board stack, which is a 24 layer construction. Since it is
in the core material it may be related to glass non-wetting of the resin
or poor glass treatment.
I'd also like to know if this is something we can consider developing
criteria for in the next generation of IPC-6012/A-600 when we meet in Las
Vegas in a couple months.
Regards,
John Perry
Technical Project Manager
IPC - Association Connecting Electronics Industries(r)
3000 Lakeside Drive # 309S
Bannockburn, IL 60015-1249 USA
+1 847-597-2818 (tel)
+1 847-615-7105 (fax)
+1 847-615-7100 (Main)
[log in to unmask]
www.ipc.org
[attachment "Bundle crack.ppt" deleted by Lance A Auer/US/Raytheon]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|