You should watch X7R ceramic capacitors especially. Different divisions of
our company have different requirements for minimum component to Vscore,
but all have larger spacing for X7R's than other SMD's. I guess they are
more brittle than the average SMD and tend to crack when the boards are
singulated if too near the Vscore. Our conservative division uses .280 for
X7R and .140 for all other. Another uses .030 and .100.
-Chris Ball
==========================
From my experience, you need a minimum of 0.025" clearance to board edge
for
v-cut. Also, our depanelization tool
requires a minimum of 0.115" clearance on one side.
=====================
Hi,
Can some tell me what is the distance for SMD components placement from
edge
of board. (V-scored panel to be separated by automatic cutter). If possible
give any reference of IPC standard.
Thanks
Narinder Kumar
Rich Schutz <[log in to unmask]>@IPC.ORG> on 05/23/2001 11:13:17 AM
Please respond to "DesignerCouncil E-Mail Forum."
<[log in to unmask]>; Please respond to [log in to unmask]
Sent by: DesignerCouncil <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [DC]
From my experience, you need a minimum of 0.025" clearance to board edge
for
v-cut. Also, our depanelization tool
requires a minimum of 0.115" clearance on one side.
Narinder Kumar <[log in to unmask]> on 05/23/2001 08:46:34 AM
Please respond to "DesignerCouncil E-Mail Forum."
<[log in to unmask]>;
Please respond to Narinder Kumar <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Rich Schutz/perry/apscoinc)
Subject: [DC]
Hi,
Can some tell me what is the distance for SMD components placement from
edge
of board. (V-scored panel to be separated by automatic cutter). If possible
give any reference of IPC standard.
Thanks
Narinder Kumar
Product Engineering
CMAC Invotronics Inc.
365 Passmore Ave.
Scarborough, ON M1V 4B3
Phone 416 321 3085 X245
Fax 416 321 3126
_________________________________________________________________________
Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com.
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET
DesignerCouncil
NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|