DESIGNERCOUNCIL Archives

October 2005

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
DesignerCouncil <[log in to unmask]>
Subject:
From:
Dee Stover <[log in to unmask]>
Date:
Wed, 19 Oct 2005 08:42:09 -0700
Content-Type:
text/plain; charset="us-ascii"; format=flowed
X-To:
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, Dee Stover <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hi all,

I have a list of flex manufacturers but I would really like some
recommendations.

Currently just a 2 layer with stiffeners - prototype quantity is really all
we will ever do.  8 mil trace 7 mil space.

Have a great day!




Dee Stover  [log in to unmask]
Sr. Tech Associate Elect
National Optical Astronomy Observatories
www.noao.edu

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2