DESIGNERCOUNCIL Archives

February 2007

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
DesignerCouncil <[log in to unmask]>
X-To:
Date:
Thu, 8 Feb 2007 11:57:10 -0800
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, [log in to unmask]
Subject:
From:
George Patrick <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (89 lines)
Looks like it to me, unless they want to pay extra for the ENIG just to
have it disappear when the solder plating is applied.  I would call them
:)

-- 
George Patrick
Tektronix, Inc.
Central Engineering, EDS Applications Support
P.O. Box 500, M/S 39-512
Beaverton, OR 97077-0001
* 503-627-5272 (voice)     * 503-627-5587 (fax)
http://www.tektronix.com    http://www.pcb-designer.com
 
"Off-Grid and Proud of it!"


-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
James Jackson
Sent: Thursday, February 08, 2007 11:53
To: [log in to unmask]
Subject: [DC] Contradictory Fab Notes?


Okay folks,

We have a client that we have contracted to fabricate a PCB for.

They finally produced a Fab Drawing, and in the Notes, they have the 
following...

3.2 Board Material to comply with IPC 4101/21,
    FR4 Material. Copper Clad both sides, 1Oz
    Copper, 0.062 Thk, ENIG Plating finish.

...

3.9 Electro Solder Plate entire copper surfaces,
    .0003 minimum thickness and reflow solder
    (Infrared Fusing Preferred).

....

Now... to my way of thinking, they have specified the PCB finish twice. 
In 3.2, they are wanting a gold finish (Electroless Nickel Immersion
Gold).
In 3.9, they are wanting a solder-plated finish.


Or, am I mis-reading this?

(I have left out the other notes 3.1, and 3.3 - 3.8, as they do not
apply to 
this.)

Could someone more knowledgeable set me straight?

Regards,

James Jackson
Oztronics 

------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
---------

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2