David,
I have always had great quality on difficult boards using Marcel
Electronics International (MEI). I have found when others say they can
do it MEI has always proven it and can back up what they do with real
quality. Up front engineering, process control and inspection is
something that MEI built it reputation on and customers, like myself,
have come to expect from them. I will not call out names but I have had
problems with other well know vendors controlling process and not doing
the proper inspections. I can honestly say, backed up by hundreds of
third party micro-sections, that if you want quality then you should at
least try MEI.
My MEI Contact:
Paul Dietenhofer
781-871-2415
[log in to unmask]
www.mei4pcbs.com
Thanks
Tony Cosentino
Tekelec - Printed Circuit Design Engineer
[log in to unmask]
www.tekelec.com
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
David Baldwin
Sent: Thursday, February 02, 2006 6:19 PM
To: [log in to unmask]
Subject: [DC] 15:1 Aspect Ratio Board Shop
Fellow IPC Members:
We are looking for a reasonably priced (I didn't say cheap, quality is
always priority) board shop that can handle a 15:1 aspect ratio. Our
current scenario is 0.180" thick 0.012" drill, 18 layers, 0.007" trace
width, 1oz. cu and 50 ohm impedance throughout.
Any recommendations are greatly appreciated.
TIA
David Baldwin CID+
______________________
Baldwin Tech Institute LLC
1736 S. Nevada Way
Mesa AZ 85204
(480) 539-4400
www.Baldwin-Tech.com
------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF
DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL) Search previous postings at: www.ipc.org >
On-Line Resources & Databases > E-mail Archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|