DESIGNERCOUNCIL Archives

September 1997

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
DesignerCouncil <[log in to unmask]>
Subject:
From:
Diseno de Cableado Impreso <[log in to unmask]>
Date:
Tue, 9 Sep 1997 22:49:37 -0600
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Reply-To:
"DesignerCouncil Mail Forum." <[log in to unmask]>, Diseno de Cableado Impreso <[log in to unmask]>
Parts/Attachments:
text/plain (43 lines)
 Hi there,

  I'm going to share with you our sistem to manufacture double sided PCB's 
to find a way of improve this sistem

1.- Drilling of the panels
2.- Electroless Copper 
3.- Electrolitic Copper 
4.- Printing of the etching mask
5.- Electrolitic Tin-Lead 
6.- Strip of the alkaly ink
7.- Etching
8.- Stripping of the electrolitic Tin-Lead
9.- Solder Mask

My question is ¿How is possible that we have to put Electrolitic Tin-Lead to
protect the PTH
from the etching end after that have to stripping?

  I'm sure that it has to be an other way to do this without wasting time
and money in
Electrolitic Tin-Lead.

  I will appreciate a lot if anyone of you can tell me your oppinions of this.

  Best regards

Artemio Martinez
Engineering Department
Diseño de Cableado Impreso

  We are using elecroplating Tin-Lead and  the mayor
problem is calculate the area to be electrplated to calculate
the current per panel.

  If anyone of you knows a software that calculate this area
please tell me where I can get it.

    Thanks for your time.

  Eduardo Tovar