DESIGNERCOUNCIL Archives

August 2002

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
DesignerCouncil <[log in to unmask]>
Subject:
From:
Matthew Lamkin <[log in to unmask]>
Date:
Fri, 9 Aug 2002 08:22:23 +0100
MIME-Version:
1.0
X-To:
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, Matthew Lamkin <[log in to unmask]>
Parts/Attachments:
text/plain (140 lines)
One potential problem is that the paste/solder underneath the component can
push the body up, so that bad joints can occur.

Another could be that the solder can be "squished" all over the place and
potentially short.

However, if its not been a problem with the assembly department and has not
caused any returns then what the heck.

The easiest way to prevent any problem would be to simple replace the solder
paste screen with one that does not include the smaller
footprints pads. And have the old one for when it is used.

Matthew Lamkin.

> -----Original Message-----
> From: Steve Kingdon [SMTP:[log in to unmask]]
> Sent: Thursday, August 08, 2002 9:28 PM
> To:   [log in to unmask]
> Subject:      Re: [DC] Land Pattern within Land Pattern (TQFP)
>
> Hi,
>
> Could someone enlighten me as to the potential problems of having reflowed
> paste under the body of an IC. I am assuming if the paste contacted the
> body of the IC, problems could occur...., but what sort of problems.
>
> We have one case where we have a SO8 inside a SO8W package. This was done
> by engineers at my company, before they had PCB designers. I looked at it,
> and didn't like it much. I asked our factory about it, but they have no
> concerns, so I left it alone.
>
> Regards,
>
> Steve
>
>
>
> Date sent:              Wed, 7 Aug 2002 13:54:42 +1000
> Send reply to:          "(Designers Council Forum)"
> <[log in to unmask]>,
>         Dom Bragge <[log in to unmask]>
> From:                   Dom Bragge <[log in to unmask]>
> Organization:           Klaxon IQA
> Subject:                Re: [DC] Land Pattern within Land Pattern (TQFP)
> To:                     [log in to unmask]
>
> > > "Robert M. Wolfe" wrote:
> > >
> > > I have a situation where there is a need to provide a dual
> > > footprint pattern for an alternate package.
> >
> > > Or would using an OSP coating solve the problem, but I guess that
> > > coating once gone would leave exposed copper under that part.
> >
> > I would tread very carefully leaving just an OSP over bare Copper in the
> > long term.
> >
> > When having done dual footprints before because of single sourced parts,
> > I've found using some sort of HASL with two different paste masks to be
> a
> > good solution. Well, at least designing two paste masks & getting the
> one
> > first needed made - the other paste mask design is then your fallback
> > solution. Also, if you are considering Alpha Levelling or other non
> > tin/lead surface treatments, then look at the long term consequences. If
> > you are doing it for a fallback solution, you could maybe do it by
> > designing in the alternate footprint but leaving the second footprint
> > covered by solder mask. Not quite as interchangeable, but you could
> > generate two topside solder masks as well as paste masks & still be able
> to
> > use OSPs etc. It depends on how you'll handle the data for future use &
> > whether you stockpile PCBs or get them JIT.
> >
> > I concur that you shouldn't screen solder paste *under* a component that
> > doesn't use it.
> >
> > --
> > Dom Bragge  CID         "The pink building"
> > Production Manager      Level 1, IBC Bldg
> > KLAXON IQA              Australian Technology Park
> > bh+61-2-9209-4404       Eveleigh 1430 NSW
> > fx+61-2-8374-5030       (Sydney, AUSTRALIA)
> > www.klaxoniqa.com
> >
> >
> --------------------------------------------------------------------------
> -
> > ------ DesignerCouncil Mail List provided as a free service by IPC using
> > LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with
> > following text in the BODY (NOT the subject field): SIGNOFF
> > DesignerCouncil. To set a vacation stop for delivery of DesignerCouncil
> > send: SET DesignerCouncil NOMAIL Search previous postings at:
> www.ipc.org >
> > On-Line Resources & Databases > E-mail Archives Please visit IPC web
> site
> > http://www.ipc.org/html/forum.htm for additional information, or contact
> > Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> >
> --------------------------------------------------------------------------
> -
> > ------
>
>
> -------------------------------------------------------
> Steve Kingdon            27 Nazareth Avenue
> PCB Layout Engineer      PO Box 8011
> Allied Telesyn Research  Christchurch
> phone +64 3 339 9223     New Zealand
> fax   +64 3 339 3002
> email: [log in to unmask]
> web: http://www.alliedtelesyn.co.nz/
> -------------------------------------------------------
>
> --------------------------------------------------------------------------
> -------
> DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To set a vacation stop for delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2