Leonard;
The only large company to use via in land on a regular
basis is Lucent, they have the process down pat.
The trick is to figure how much solder you going
to lose to the hole.
It real helps on high density boards.
Lou
Leonard Toohey wrote:
>
> What is the state of the industry regarding putting
> vias in the center of SMT discrete device pads?
>
> I am mainly wanting to know about 0603, 0805 and 1206 devices.
> Is board thickness a factor?
> What about via hole size?
>
> Thanks,
>
> Leonard Toohey
> [log in to unmask]
> 12303 Technology Blvd.
> Austin, TX 78727
> Ph(512) 257-5423
> Fx(512) 249-7236
> http://www.netspeed.com
>
> ################################################################
> DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE DesignerCouncil <your full name>
> To unsubscribe: SIGNOFF DesignerCouncil
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
--
Lou Dallara Techno Visionary
"We have it in our power to begin the world again."
-Thomas Paine, Common Sense (1776)
http://www.waterw.com/~ldallara http://www.arcosanti.org
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|