I also read the IPC-A-610 10.5.2 Conformal Coating
William Brooks, CID+
Printed Circuit Designer
Nordson Asymtek
2747 Loker Avenue West
Carlsbad, California 92010-6603 USA
TEL: +1.760.930.7212
CEL: +1.760.216.0170
[log in to unmask]
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Brooks, William
Sent: Friday, April 07, 2017 3:10 PM
To: [log in to unmask]
Subject: Re: [DC] Conformal coating notes?
I found:Mil-I-46058C 1972 - Insulating Compound, Electrical (For coating Printed Circuit Assemblies)
So I would want type AR - Acrylic Resin
Also found: NHB5300.4(3J) referenced in the IPC-D-325 example assembly drawings
Looks like that was a NASA spec.
Also noted reccomendations of Humiseal 1B31 and Humiseal 1B73 in a presentation I found online...
Any comments on either?
How should my notes read?
William Brooks, CID+
Printed Circuit Designer
Nordson Asymtek
2747 Loker Avenue West
Carlsbad, California 92010-6603 USA
TEL: +1.760.930.7212
CEL: +1.760.216.0170
[log in to unmask]
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Brooks, William
Sent: Friday, April 07, 2017 1:31 PM
To: [log in to unmask]
Subject: [DC] Conformal coating notes?
Does anyone have standard notes for conformal coating on printed circuit boards?
I'm thinking Acrylic for its ease of application and rework ability.
William Brooks, CID+
Printed Circuit Designer
Nordson Asymtek
2747 Loker Avenue West
Carlsbad, California 92010-6603 USA
TEL: +1.760.930.7212
CEL: +1.760.216.0170
[log in to unmask]<mailto:[log in to unmask]>
---------
This email is intended only for the use of the party to which it is addressed and may contain information that is privileged, confidential, or protected by law. If you are not the intended recipient you are hereby notified that any dissemination, copying or distribution of the email or its contents is strictly prohibited. If you have received this message in error, please notify us immediately, by replying to the message and deleting it from your computer. WARNING: Internet communications are not assured to be secure or clear of inaccuracies as information could be intercepted, corrupted, lost, destroyed, arrive late or incomplete, or contain viruses. Therefore, we do not accept responsibility for any errors or omissions that are present in this email, or any attachment, that have arisen as a result of e-mail transmission.
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL) For additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
This email is intended only for the use of the party to which it is addressed and may contain information that is privileged, confidential, or protected by law. If you are not the intended recipient you are hereby notified that any dissemination, copying or distribution of the email or its contents is strictly prohibited. If you have received this message in error, please notify us immediately, by replying to the message and deleting it from your computer. WARNING: Internet communications are not assured to be secure or clear of inaccuracies as information could be intercepted, corrupted, lost, destroyed, arrive late or incomplete, or contain viruses. Therefore, we do not accept responsibility for any errors or omissions that are present in this email, or any attachment, that have arisen as a result of e-mail transmission.
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL) For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
This email is intended only for the use of the party to which it is addressed and may contain information that is privileged, confidential, or protected by law. If you are not the intended recipient you are hereby notified that any dissemination, copying or distribution of the email or its contents is strictly prohibited. If you have received this message in error, please notify us immediately, by replying to the message and deleting it from your computer. WARNING: Internet communications are not assured to be secure or clear of inaccuracies as information could be intercepted, corrupted, lost, destroyed, arrive late or incomplete, or contain viruses. Therefore, we do not accept responsibility for any errors or omissions that are present in this email, or any attachment, that have arisen as a result of e-mail transmission.
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|