DESIGNERCOUNCIL Archives

June 2007

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Denis Lefebvre <[log in to unmask]>
Reply To:
(Designers Council Forum)
Date:
Tue, 5 Jun 2007 07:21:11 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
The symptoms sound exactly like a barrel crack from Z-expansion. 

Something to look for... If inner layers are planes, were non-functional
pads retained to minimize resin-rich stack-up around PTH's?  

Denis Lefebvre, CID+
Sr. PCB Designer
Finisar Corporation
(408)542-3832

-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Tom
Parkinson
Sent: Tuesday, June 05, 2007 7:14 AM
To: [log in to unmask]
Subject: [DC] Via Open

Tech Net & Designer Net

Greetings. We are running into a situation on Lead Free processed PCBs.
Failure mode is finding open vias during unit testing (fully populated).

Boards are Tg170, Material type EM320, 0.063" thick boards.  
6 layers of 1 oz copper. ENIG 3~5u"

Suspect vias go from top layer to bottom layer only.

After running through reflow, we have found vias open. No visual signs
of delamination, however when ohming out the via, if we press on the via
we get continuity - thus we suspect the vias are opening during the
process.

Anyone out there having these problems, or information concerning this
failure mode?  Z-expansion failure?


Tom Parkinson
Quality System Manager - CIT
WinTronics, Inc.
Phone: 724-981-5770 - extension 235

------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF
DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL) Search previous postings at: www.ipc.org >
On-Line Resources & Databases > E-mail Archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
---------

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2