DESIGNERCOUNCIL Archives

June 2004

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
DesignerCouncil <[log in to unmask]>
X-To:
Designers Council Forum <[log in to unmask]>
Date:
Fri, 25 Jun 2004 08:46:52 -0700
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, "Mitch S. Morey" <[log in to unmask]>
Subject:
From:
"Mitch S. Morey" <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain;charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (99 lines)
Hi Tom,

Is for high volumn fab and assy? For fab it's not a problem. With Assy it
could turn into a very large problem depending upon what steps you're
taking to ensure "flatness" of the BGA pad with the via-in-pad design. The
company I work for is seeing not a lot, but enough fallout with the BGA
assy (opens) to completely eliminate VIP designs. One way we're doing it
is to stay away from 'less than 1mm' BGA packages. One way we've also
experimented is to 'stagger' the uVia slightly off the BGA pad. That way
the majority of the BGA pad will be completely flat even if the VIP area
is not. (Yes, we've also experimented with solderpaste volumn too, but
that's again just a cludge work-around to solve a fallout anomaly)

Again, this is High Volumn only. There are many, many, many companies
where it's not a concern, or have solved the issue to their satisfaction
(maybe they have better assy equipment/manufacturers)

Good day.

Mitch
>
> If "Via in Pad" refers to laser microvias, this is a fairly common
> practice,
> and likely everyone owns a product (digital camera, cell phone, camcorder)
> than uses this type of design.  If properly designed and fabricated you
> should have no problems manufacturing the assembly.
>
> Check the DC archives, as there's probably a wealth of information on the
> subject.
>
> Dave
>
> -----Original Message-----
> From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Tom
> Parkinson
> Sent: Friday, June 25, 2004 10:14 AM
> To: [log in to unmask]
> Subject: [DC] VIA in Pad
>
> We're a CM.  One of our customers is asking us to build a board assembly
> that will be using BGAs with VIAs in pads.  They are in the design stages
> at
> this point, and we have some concerns with having a Via in the middle of a
> BGA pad.  Anyone have suggestions and/or experience with this??
>
> Thanks
>
>
> Tom Parkinson - Quality System Manager - CIT
> WinTronics, Inc.
> Ph: 724-981-5770 Ext. 235
> Fax: 724-981-1772
>
>
> ----------------------------------------------------------------------------
> -----
> DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To set a vacation stop for delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ----------------------------------------------------------------------------
> -----
>
> ---------------------------------------------------------------------------------
> DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To set a vacation stop for delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
>



-----------------------------------------
This email was sent using http://cafemail.pcbcafe.com .

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2