The inner layers may have more of a registration problem, due to shifting
during lamination. You might want to add some extra clearance to you standard.
>In this same vein -- We have traditionaly used anti-pads which are larger
>than the positive pads on the outer layers. I have thought about switching
>to an anti-pad just large enough to clear the hole barrel + std clearance.
>Any comments/advise?
>