This has been very useful, thanks everybody! In the early days we used sample boards with a variety of components to prove we can get around component height/ corner/ shadowing issues and all of our tests proved our coating was spot on, and on every batch our first off is checked with an eddy tester, we've never had a situation where we've had to strip/ re-apply the coating due to it being insufficient. Thanks again!