Dear Technetters.. Although this subject has received much attention lately, nobody has mentioned the problem I find very strange: Sometimes, the nickle thickness approaches zero along the edge of e.g. lager pads, wide tracks and solid copper planes. It is always the lower edge of the affected area. I suspect some sort of hydraulic effect in the bath to cause it, but have never found the answer. It mainly affects boards on some kind of Teflon material, although is as been observed on Polyimide and FR4 as well. Plasma has been tried, hoping that altering the surface properties would make a difference. No effect found. Chemistry is from Shipley/Ronal. Hoping someone out there has a clue.... regards Torben Østeraa Printca AS [log in to unmask] <mailto:[log in to unmask]> ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################