Geoff, Most laminates are pressed at higher pressures and temps.Almost anything will work other than specialty materials. Mike Doty P.E. Hadco TCE ______________________________ Reply Separator _________________________________ Subject: [TN] laminate in hot oil Author: Geoff Layhe <[log in to unmask]> at smtplink-hadco Date: 12/1/99 5:00 PM Here's a strange request, I,ve been asked to specify a copper clad laminate for a circuit board which will be immersed in hot oil (80ºC) at 3000psi pressure. Anybody got any ideas? Geoff Layhe www.lamar-uk.co.uk ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################