revenons a nos moutons Brian, We have been running 10 cells for about 2&1/2 years now. Biggest motivation for switching was throughput and surface distribution particularly on smaller surface features. Our target is 1.3 mils in the hole & 1.2 on the surface in 70 mins.. We do this on .093" bds wt .010" holes in a 20 year old bare bones no options automatic. Haven't really had the time nor need to test much higher than that. However, there are definite limits to what it can overcome for any particular cell setup, Ground Planes, isolated traces, high aspect ratios, etc. Since many of these things can not be adjusted, you have to experiment to find a happy median for most things and what the real limits are for the rest. Hope this answers your original question. 1. Benefits a. shorter cycle times on difficult jobs b. less surface copper on isolated features = less copper and LPI usage c. ability to run finer spaces without resist lock-in d. for myself the most important; more copper in the holes = more robust vias 2. Disadvantages? a. higher additive cost, minor + should continue to come down? b. capital - 9-12 month ROI just in material savings? c. can't have any marginal connections/bussing, only good or bad boards? Lurking in the background Welch -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of brian carlson Sent: Wednesday, November 24, 1999 11:19 AM To: [log in to unmask] Subject: [TN] Pulse plating Technet, Can someone give me an insight on benefits or possible disadvantages to pulse plating. I am interested to hear some stories of what happens to the Cu thickness in the hole wall when aspects ratios increase to 15:1. Any feedback is welcome. Rgds, Brian Brian Carlson Technical Support Engineer Yamamoto Mfg. (USA), Inc. (408)944-8368 (Office) (800)514-6246 (Pager) (408)944-1361 (Fax) ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################