Hi to all, I was totally confuse by the OSP & Entek 106A finishing. What is the difference between OSP & Entek 106A? In term of :- 1) Cost 2) Electrical performance 3) Process issue 4) Stencil thickness Thanks! Adeline Ko ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################