hi, as you are probably aware, cotton fiber, as well as wood, is cellulose based. phil crepeau -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Sunday, December 19, 1999 6:02 PM To: [log in to unmask] Subject: [TN] Blue cotton buffer paper and recycling - mistake! mistake! Hi Technetters, I made a mistake! Cotton based buffer paper is of course COTTON based and not cellulose based. Cellulose is the normal paper or craft paper based material. Cotton beside buffer paper also used for banknotes (still waiting for feedback from North Korea and Cuba on that - just kidding) Again, if YOU use cotton based buffer paper for laminate or multilayer pressing what you do with it? Just through it away? Jens Behrens -- Sent through Global Message Exchange - http://www.gmx.net ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################