Hi Scott, Mil-Std-883E doesn't have the product requirement, but the test method for solderability (Method 2003) does have a test requirement: "4.4.1 Solder dipping of gold plated terminations. Gold plated terminations shall be cycled twice in flux and solder using one or two solder pots. The first immersion is to scavenge the gold on the terminations. It is recommended that a separate solder pot be used for gold plated devices." Hope that helps, Glenn Scott A. Bowles <[log in to unmask]> Wrote: | | TechNetters, | Can anyone point me to a test method in MIL-STD-883 that deals with gold on | Military assemblies. I have an understanding that from back to the 60's, | boards built for Military applications are not to have gold on them or | actually in the solder joints. And if they do, then they must be double | dipped/tinned or something to get rid of the gold. Any help is greatly | appreciated. | Thanks, | Scott ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################