Hi Stella, > ---------- > From: Neyman, Stella[SMTP:[log in to unmask]] > > PCB designers please help! > We are designing 2 oz copper PCB with the plain which suppose to carry 30 > amps. > 1. How many vias would be necessary to transfer 30 amps from one side to > another? > With a via diameter of .031", with 1 oz copper in the via (ignoring overplating with solder), the equivalent cross section in square mils is 2Pi(15)(1.4) = 132 sq. mils. This cross section can carry approximately 4 amps with a 10 degree (C) rise in temperature above ambient. Therefore, you would need at least 8 vias this size. The more vias you use beyond 8, the lower the impedance from side to side. Low impedance from the power supply (and ground!) is important for the function of analog and high speed circuits. > 2. Does the via need relief (wagon wheel) or may be solid? > Thermal relief is only necessary when soldering a lead to a pad or a plated through hole. Thermal reliefs are not required (or even desirable) on power or ground vias. Some people use them to verify by sight, when viewing artwork plots, what is connected to the plane. > 3. What should be the via size (0.020" or 0.031") > With an .020" via, the equivalent cross section in square mils is 2Pi(10)(1.4) = 88 sq. mils. Each via will then carry about 3.5 amps with a 10 degree (C) rise in temperature above ambient. Obviously, you'll then need to use 9 vias (minimum) to carry 30 amps. Michael Hiteshew Lockheed Martin Launching Systems [log in to unmask] (410) 682-1259 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################