Vinit check IPC archives ; wrote about it more than enough . We still dispense all of our small volumes and prototypes , also inline dispensing adds to stencil where we need more paste on the pad/hole, (cures cap thombstoning instantly , for example) As far as validations, being FDA controlled, you're on the right address : Top gun in paste after all process criteria (it wicks nicely) and cyclings (7 months to IPC-SM-785, 0-100'C)is : indium NC-SMQ90, -400+500mesh, ask indium folks for ResMed's 200gms syringe (you'll need 20-25psi to move it), or standard 50gms (too many changes and purges in long runs , you need 7-10psi [constant]) cu Paul Klasek http://www.resmed.com thanks for the box Inge , when you'll publish the silver polymer concluding specs ? -----Original Message----- From: Ingemar Hernefjord (EMW) [mailto:[log in to unmask]] Sent: Thursday, 4 November 1999 0:21 To: [log in to unmask] Subject: Re: [TN] Solder Paste Dispensing Vinit, try this voice number: +46 8 757 4901, ask for L.A. Olofson, he has been in the game for 20 years, I guess he can give you advice. Or wait for ResMed's answer, as they live 'just around the corner' for you. /Ingemar Hi Technetters, I am using Panasert GLue Dispenser HDP-III. Recently one of my PCBs has been changed to double sided one with reflow on one side. I donot want to invest on a solder paste printer since the volumes are not so high at this moment. Has anybody tried solder paste dispensing using a glue dispenser. What type of solder paste is to be used. (Any vendors qualified???) Any information will be highly appreciated. Regards Vinit Verma National Panasonic India Ltd. 510, International Trade Towers, Nehru Place Tel: +91-11-6292870-74 Fax: +91-11-6292877-78 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################