Hans, We sometimes use Dynasolve 220. Call Dynaloy, Inc at 800-669-5709 or 317-788-5694 for a recommendation. Humiseal 1090 is a stripper for silicone coating which might also work for your application. Talk with Jim Laurence at Humiseal for a recommendation (718-932-0800). Regards, Mary Davis Mary M. Davis Materials & Process Engineering ELDEC 425-743-8327 FAX 425-743-8562 [log in to unmask] ---------- From: Hans Shin [SMTP:[log in to unmask]] Sent: Friday, November 05, 1999 2:17 PM To: [log in to unmask] Subject: [TN] The following question is related to analytical chemistry: Does anyone know of any solvents that will dissolve/digest a cured RTV (silicone elastomer, polydimethylsiloxane, dimethicone, etc.) material (excluding hydrofluoric acid)? Hans Shin ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################