If they used electo plated gold the brown pads may be isolated circuits that are not connected to the plating system. The brown will be immersion gold attached from their bath. Probably not very thick. Chuck Brummer Acuson Ken Patel wrote: > Guys, > I have received a Nickel-Gold fab from my fabricator and found some randomly > located brown pads, missing shining gold finish. > > What kind of defect is this? Is it ok to proceed assembly with the this kind > of defect? Any reliability concerns? > > re, > ken patel > > ______________________________________________________ > Ken Patel Phone: (408) 490-6804 > 1708 McCarthy Blvd. Fax: (408) 490-6859 > Milpitas, CA 95035 Beeper: (888) 769-1808 > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################