A supported hole is plated through...an unsupported
hole is not.
Bill Gilman C.I.D.
Radio Systems
Corp
Technetter,
In many IPC standards, the term
'Supported hole' is often used. Could
anyone
tell me what's the difference between supported hole,
and
plated through hole?
Thanks.