In a message dated 09/01/1999 7:58:00 AM Central Daylight Time, [log in to unmask] writes: << Steve, What are the problems with trying to wave solder 0402s? Do they fall off the board or result in insufficient fillets or what? Wade Oberle>> Hi Wade, It's trying to get the epoxy in between those two teeny-tiny pads buddy...that's the problem! -Steve Gregory- ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################