Lenny Be aware the ammoniacal etchant is considerably more expensive per ounce of copper etched than is cupric chloride. Also, ammoniacal can use solder as an etch resist, cupric cannot. Jerry Sallo Sallo Consulting Services [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################