Morning, Werner, as you have an eye on most of what happens on this planet, I must ask you: who makes Cs and Ls and Rs like <1206> with FlipChip bumps, 2 or more on each termination. For getting a standoff. Special need. C4-like. Must be taped. CU Ingemar Hernefjord Ericsson Microwave Systems -----Original Message----- From: Werner Engelmaier [mailto:[log in to unmask]] Sent: den 3 september 1999 23:02 To: [log in to unmask] Subject: Re: [TN] Hi Grant, Unless your application is for a severe use condition, putting 1206 caps on 0805 pads does not affect solder joint reliability; in fact, since the fillets do not pull the caps down you might have a greater solder joint height and get better reliability. Also, without solder fillets you are much less likely to get cracked caps. Werner Engelmaier Engelmaier Associates, L.C. Electronic Packaging, Interconnection and Reliability Consulting 7 Jasmine Run Ormond Beach, FL 32174 USA Phone: 904-437-8747, Fax: 904-437-8737 E-mail: [log in to unmask], Website: www.engelmaier.com ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################