TechNet'ers: Pat Brooks ask a good question about the plating method, which I missed in my original question/info e:mail thing-a-ma-bob. And the answer is . . . Can you tell it's Friday? . . . electroless Nickel and immersion gold is the plating method. All have a great weekend. Ron -----Original Message----- From: Hollandsworth, Ron Sent: Thursday, September 16, 1999 3:12 PM To: [log in to unmask] Subject: Subj: Poor Wetting/Solderability/Contamination/???? Importance: Low Good Day TechNet: I am experiencing poor wetting, insufficient hole fill, and what appears to be phosphorus contamination. Some details are: 1. Happening/Noticiable after wavesolder operation. 2. Wavesolder setup is: 230 F top side board temperature, Low Residue VOC Free Water Based Flux by Kester, minimal to no solder balls (appears flux/preheat has sufficient timing), conveyor speed at 3 ft. per minute, and spray fluxer with pitch/pressure/speed control (good coverage). 3. Handsoldering seems to work, however, may have selected boards that are solderable. 4. Connector leads are within tolerance and board is within tolerance, however, at max and min tolerance the lead protrusion left is minimal. Believe it acts like a plug, however, defect characteristics appear on bottom side of board. 5. Nickel/Gold board - electroless plating 6. Relatively fine pitch connectors, however, larger .050 mil connector has shown poor wetting, insufficient, cantamination, etc., as well as randomly other parts of board. 7. Boards are not stored for a long time before use. Cycle time very short from dock to line. I noticed that last week someone else had a problem that is about the same as this. We have also tried paste-in-hole for the connectors and it appears to help significantly, but there is still a problem, still you should be able to wavesolder these boards and not add an extra step in the process. Good topic, I think. Has any one solved this issue or speculation on how to solve it. I read the speculations, but it appears to be plaguing other besides just us at the present time. Plus it comes and goes. Looking for clues????? Ron Hollandsworth Ops Task Leader ITT [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################