Clive, it is not quite possible to prevent the static prior ; the tapes separation mainly generate the charge ; if you'd like something more down to earth perhaps a grounded bar/chain curtain/etc ; with the empty tapes traveling over ? On the cost side ; as you know what you did pay for your carbon bins : calculate how much of this expensive material you discard over the year as per your wish ; and you find instant global shortage of dissipative materials and excessive expense . Paul Klasek ResMed -----Original Message----- From: Clive ffitch [mailto:[log in to unmask]] Sent: Friday, 10 September 1999 20:21 To: [log in to unmask] Subject: Re: [TN] ESD and SMT Tape/Reels - Concern All, Thanks to everyone who replied to my recent posting re the excessive levels of ESD build up on component tapes and reels. We at least are not the only ones who have concerns in this direction, either here in the UK or elsewhere. The use of ionisers etc may be a solution, as many indicate is for them, but this is really only a curative solution for a problem that should in fact be prevented in the first place, before it gets to us. In other words, such parts (supplied in non-ESD protective tapes and reels) that are for use in ESD protective areas for electronics assembly/pick & place - where more sensitive ESDSs are susceptible to damage - should be supplied to us using ESD-SAFE materials. After all, that is what we expect of other materials supplied to our assembly areas - totage and the like - and there is a substantial industry now catering to such needs that an ESD protective material property should now be a selling point/plus point. So if there are any component tape/reel suppliers out there on TechNet, why aren't they? For our part, we will be raising this issue at industry forums here in the UK, some of which have component suppliers involved within the various working groups. We may only order a small number of parts on our own, but if we all ask for what we really want, there is a chance we may actually get it. Market demand and all that. Clive ffitch MBUK England ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################