Eric , Did you envision any through features? what would be the operating specs, IE rough temp range, and frequency. It is possible to make them very thin , however sacrifices must be made. Russ Smith ---------- From: Brett Goldstein To: [log in to unmask] Subject: Re: [TN] Info on Ceramic PCB's needed Date: Tuesday, August 31, 1999 12:29PM I've seen 11 mil thick, 2 layer ceramic circuits - but you have to handle them very carefully, as they break easily. Brett Goldstein EVI, Inc. > I need to know how thin a 2 layer ceramic PCB could be. I'd also like to > find out who makes them. > > Can anyone help? > > Thanks, > > > > Eric Christison > Mechanical Engineer > VLSI Vision Ltd > Aviation House > 31 Pinkhill > Edinburgh > EH12 7BF > > Tel: +44 (0) 131 539 8165 > Fax: +44 (0) 131 539 7141 > A company of the STMicroelectronics Group > ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################