Hi Stefania, Don't know the details but you might look at new racks. We bought some Teflon coated ones from M & B which don't plate up. Let me know if you (or anybody else) wants contact info. Hans ~~~~~~~~ Hans M. Hinners WR-ALC/LYPME Bldg. 640 Materials Engineer 380 Second Street, Suite 104 Manufacturing Eng. Sec. Robins AFB GA 31098-1638 912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax) [log in to unmask] > Does anybody know an electrochemycal stripping solution > for tin-lead and copper on the racks? > Thanks in advance, > Stefania ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################