Al, Those are old parts. Hmmm. Although weight loss studies I have done and have seen from vendors show most of the moisture leaves components within the first four hours, these investigations have not been with parts that have had the possibility to suck up moisture for five years. (Well they wouldn't be doing it continuously.) I personally would be a whole lot more comfortable with a 24 hour temperature soak, at the temperature you mentioned. I would expect that at this temperature you should be OK with respect to growth of surface oxide, unless of course you are right on the hairy edge of your pass/fail criteria for solderability. I would also be inclined to use them as soon as possible after they come out of the oven, as I have no idea how susceptible the particular SOICs you have are to moisture pick-up. regards, Bev Christian Nortel Networks > -----Original Message----- > From: Alan Shaw [SMTP:[log in to unmask]] > Sent: Tuesday, September 14, 1999 4:34 PM > To: [log in to unmask] > Subject: [TN] Baking SOIC packages to dry them prior to reflow solder > > I have 5 year old plastic SOIC packages on reels and want to dry them out > in > an oven rather than leave it to the pre-heat of the reflow solder machine. > Production asked for temperature and time for the SOIC to be in the oven. > My initial thoughts are to put them in a cold oven and set the thermostat > to > 110'C and leave them baking for 4 hours. Then turn off the oven. Remove > them > when cool and use in the insertion machines the next day. > Is the temperature and time suitable? > > The leads have passed a solderability test already, would the time in the > oven have a significant effect on solderabitiy? > > Al Shaw > ashaw at napcosecurity dot com > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################