Steve,
Changing the predominant culture of any company, department, corporation,
etc. is probably the most daunting task anyone can take on.
I keep a quotation directly across from my desk so that I can read it every
day. It goes
"There is nothing more difficult to take in hand, more perilous to
conduct, or more uncertain in it's success, than to take the lead in a new
order" Machiavelli.
I'm the QA Manager for a board shop. The major part of my position of
course, requires that I change the predominant culture from one of acceptable
yield loss, rework, blame and unaccountability to the extreme opposites as well
as establish and maintain a QMS that meets 9002 requirements.
I've been successful at this company, as with others. For me, the secret to
this change of culture is persistence, persistence,
persistence, persistence.
The training program I have developed here follows that simple philosophy.
Training is hardly ever performed in a classroom here. What is written in our
procedures is "continual, daily training shall be
performed" And I've made it my responsibility to follow up
continually, and daily with team leaders, supervisors, and managers to ensure
this is being performed.
You can try to smash the culture in immediate ways, but this will most
certainly lead to resentment from the workforce, and frustration for you. Or you
can take small, daily steps that over time will be far more effective.
Your situation; however, has a twist or two. Were I in your shoes I would
ask myself, if we are producing product at a higher quality level than IPC Class
II, why take a backward step, why not find a way to maintain that level
(MIL-SPEC) in the most cost effective manner. While I agree QA should not reject
product that meets specifications, they should have the responsibility and
freedom to communicate these process conditions that may eventually lead to
nonconforming product. In my opinion, dull solder joints should be flagged, the
process producing these conditions should be addressed and the condition or
variable causing it should be eliminated from the system.
Have I rambled enough? Well I hope this
helps you a little.
Good luck
Franklin
>Hey ya'll!
>
>Well, it's cooled down
to a balmy 90-degrees here, and boy are my sweat
>glands
happy!...hehehe
>
>But email ain't to talk about my how much I
perspire, but about changing
>cultures. One of my
"opportunities" as presented to me here is figuring out
>how to
reduce costs (aren't we all trying to do that?).
>
>One of the
things that I've noticed since I've been here, is that there is
>that
everything is looked at through MIL-SPEC shaded glasses...and I've
found
>that boards we were building under IPC 610 class-II standards were
being
>touched-up un-neccessarily. Things that are maybe only a process
indicator,
>but acceptable, are being reworked. For one example, dull
solder joints that
>were caused because an active OA flux was left on
longer than it should have
>been before cleaning has made the joints look
dull. QA won't accept the board
>until all the solder joints are
sparkling. I'll fix the problem about the
>operators leaving the flux on
too long before washing the board, but you
>still don't need to touch
every joint up! But I sure couldn't convince QA of
>that...and so on it
goes.
>
>Part of the history here is that they've always done
MIL-SPEC work here, and
>a lot of that work isn't as plentiful as it once
was. One reason I fully
>believe is because of the costs associated with
building product to that
>level of quality. At my last company we built
product that was going on the
>space shuttle, but yet it only needed to
meet 610 Class-II standards. It
>wasn't any guidance stuff or anything
like that, but even NASA is relaxing
>things a
bit.
>
>Class-II product is something new here, and I think I'm
gonna have my hands
>full trying to get people out of that MIL-SPEC
culture...it'll be hard to
>make any money doing things that way with the
difference in the margins
>between MIL-SPEC and commercial class-II
product..
>
>Any suggestions anybody?
>
>Thanks
ya'll!
>
>-Steve
Gregory-
>
>##############################################################
>TechNet
Mail List provided as a free service by IPC using LISTSERV
1.8c
>##############################################################
>To
subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your
full name>
>To unsubscribe: SIGNOFF
TECHNET
>##############################################################
>Please
visit IPC web site (http://www.ipc.org/html/forum.htm)
for additional
>information.
>If you need assistance - contact
Gayatri Sardeshpande at [log in to unmask]
or
>847-509-9700
ext.5365
>##############################################################
>