Hello Jos, Here at C-MAC we go by centrifuging for 5 to 50 minutes. What brand of adhesive do you use ? somertimes it makes a big difference. Manon C-MAC -----Message d'origine----- De : Jos Groffils <[log in to unmask]> À : [log in to unmask] <[log in to unmask]> Date : 26 août, 1999 06:49 Objet : [TN] bubble-free paste Hello, Not too familiar with paste handling I have to bring over adhesive from a 5 liter can to syringes of 25 or 50 ml which will be used in dispensers. How can I do this without mixing air in the rather viscous (15 000 Pas or cP) adhesive? By centrifuging? Putting vacuum afterwards didn't help. What is normal practice? Who has this equipment? Thanks Jos BC Components ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################