In a message dated 08/23/1999 11:53:14 AM Central Daylight Time, [log in to unmask] writes: << Steve, how about using an electric eraser to remove the solder from the gold tips? You can experiment with different erasers (more or less abrasive) to see what works best for you. Don't have to worry about putting in any deep scratches by using an X-acto blade. Ron >> Hi Ron! Hmmm, might try that...these fingers that I was doing were pretty "contaminated"... like three boards were waved without masking the fingers off...DUHHHH! (Oh I was just a little bit hot when I learned that!). Might try your suggestion...get me a couple of scrap boards and give er' a go! Thanks! -Steve Gregory- ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################