Do you want to examine the alloy's structure or to remove the material from a copper circuit? Don Vischulis nishath yasmeen wrote: > Hello Everyone! > What is a good etchant for SnPb (60/40) Solder? > Thanks, > Yasmeen ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################