Hello All We have 50-mil pitch two row TH connectors on some of our boards. The direction of flow in wave is parallel to the row of pins. This part always bridges on the last pins as there is lot of drag at the end. We also tried to add a thieving pad at the end of the last pin in the direction of flow to help, but the test results didn't help much. (only 50% yield). Does anyone has experience with this case? Any help is appreciated Thanks Uday ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################