Type II = 99.0 percent Gold minimum Grade C= Knoop hardness 130-200, incl. Class 00 = 0.00002 inch thick, minimum > --Original Message----- > From: TPE Engineering TechNet [SMTP:[log in to unmask]] > Sent: Friday, August 27, 1999 10:50 AM > To: [log in to unmask] > Subject: [TN] Mil-G-45204 > > I have a drawing that requires keypads to be plated with > gold. This drawing references MIL-G-45204, type 2, grade C > class 00. What type of gold is this? Electrolytic, immersion > or electroless. How much nickel is required to be plated > under this gold? Any help I can get on this would be > appreciated. > Thanks, > Ron Hayashi > Toppan Electronics > 1-858-695-2222, ext. 243 > [log in to unmask] > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################