For things like that you should go to a primary source. Please contact Humiseal and ask if there is a conformal coating remover for any of their 1Bxx product. Humiseal is located at Woodside NY 718-932-0800 bobz > -----Original Message----- > From: Hinners Hans CIV WRALC/LYPME [SMTP:[log in to unmask]] > Sent: Thursday, August 26, 1999 9:04 AM > To: [log in to unmask] > Subject: [TN] Acrylic Conformal Remover which doesn't touch Epoxy? - > Does it e xist > > Hey Everybody, > > I'm looking for an acrylic conformal coating remover which won't touch > epoxy. > > I tried Kyzen's Conformox AU and it changed the physical appearance of the > epoxy - dulled it. > I should run a hardness test but I think it softened it too. > > The current plan uses Trans LC and that leaves a hazy residue. > This residue does come off when I run it through our Aqueous Cleaner or > get > the q-tips out but . . . > an extended soak in Trans LC will soften the epoxy too, so I'm highly > motivated to find an alternative. > > I'm not familiar enough with the properties of acrylic and epoxy to know > whether I'm trying to defy physics (yet!). > Somebody out there in cyberland must have faced this opportunity already. > > Hans > > 5 more days and I will have been in the Industry for 1 whole year. > > Air Force Material Command > Our mission: develop, deliver and sustain the best products for the > world's > best Air Force. > ~~~~~~~~ > Hans M. Hinners WR-ALC/LYPME Bldg. 640 > Materials Engineer 380 Second Street, > Suite 104 > Manufacturing Eng. Sec. Robins AFB GA 31098-1638 > 912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax) > [log in to unmask] > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################