You aren't going to like this! If it's Polyclad PCL-FR-370, we've had improvement in holewall texturing using several different desmear chemistries by utilizing a 2 hour postdrill bake @ 300 F. SEM's do show improved topography. I've also heard it stated that improved texturing doesn't necessarily equal improved holewall adhesion. The end product speaks for itself. -----Original Message----- From: Tony Charais [mailto:[log in to unmask]] Sent: Wednesday, July 21, 1999 6:09 AM To: [log in to unmask] Subject: [TN] Permanganate Problems We are seeing an occasional problem with our current permanganate process. We have a DOE running but we are having problems developing topography in the hole on a given product. This is a high aspect ratio multilayer board. We are confident that the problem isn't related to fluid transfer in the hole. This product is based on a PolyClad core. Has anyone else had problems with PolyClad material? We are wondering if it could be something to do with their resin. Any support from the technet would be appreciated. Tony Charais Manufacturing Engineer [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################