We always focus on the end thickness of 0.5/0.6 after scoring, with max 0.15 shift. best regards. Joachim Verhagen [mailto:[log in to unmask]] consulting engineer, EASEurope B.V. [http://www.easeurope.com] Goorseweg 5, 7475 BB Markelo, Netherlands, tel. +31 (0)547 - 367 347 > -----Original Message----- > From: DesignerCouncil [mailto:[log in to unmask]]On Behalf Of Jerry > Galang > Sent: Thursday, July 22, 1999 22:44 > To: [log in to unmask] > Subject: [DC] Scoring? > > > Greetings, > > When scoring different thickness FR4 boards should the amount of > material left > be the same (we use 0.25mm (.0984) for a 1,016 (.040) thk board)? > Today we are trying to score 1,157mm (.062) boards, so this > question popped up. > Are we thinking correctly about using the same amount of material > left after > scoring regardless of board thickness? > > > < > distance left between cuts | | = 0,25 (.01) > > Any answers would be appreciated. > Jerry Galang > Xircom > > tia > Jerry Galang > Xircom >