Barbara - Generally, the CAD file for a solder paste artwork is scaled to match the pad sizes or 5% under. It is a tool which can be adjusted by the manufacturing engineering function at whatever assembly facility deals with the product. In this manner, the product remains adjustable to fit the assemblers processes. Regards - Kelly