Jim, Make sure to use a solder paste with 2% silver, unless you like the look of grainy solder joints sure to be rejected by your quality folks. Also look at the component manufacturers reflow specs, make sure you're hitting their recommended temps for peak and time above liquidus. Mike McMonagle PCA Process Engineering Supervisor K*Tec Electronics 1111 Gillingham Lane Sugar Land, TX 77478 (281) 243-5639 Phone (281) 243-5539 Fax [log in to unmask] > -----Original Message----- > From: Jim Marsico 516-595-5879 [SMTP:[log in to unmask]] > Sent: Thursday, July 29, 1999 8:50 AM > To: [log in to unmask] > Subject: [TN] PALLADIUM SILVER FINISH > > Hello again... > > Any concerns soldering a surface mount chip component with a palladium > silver > finish? > > Thanks in advance > > Jim Marsico > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################