Jim, Ah there's the rub, in your last phrase - "if any quality issues could arise". If it were to happen, for whatever reason, each solder bar manufacturer could then point at the other. Unless you are talking a lot of solder I would recycle it or use it in a small static solder pot, not in one of your wave solder machines. regards, Bev Christian Nortel Networks > -----Original Message----- > From: West, Jim [SMTP:[log in to unmask]] > Sent: Wednesday, July 28, 1999 4:40 PM > To: [log in to unmask] > Subject: [TN] Mixing solder bars from different manufacturer's > > Hi all, > > This might be a silly question, but I received some left over solder from > a > customer that is made by a different manufacturer than what we use. Both > solder bars are 63/37 and I want to know if you can mix solder from > different manufacturers, I'm not sure if manufacturers do anything > different > with their product or if any quality issues could arise. > > Thanks, > > > Jim West > Manufacturing Engineer > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################