Hi Bill, I agree that the solder viscosity at Liquidus is too high for good flow anywhere, let alone capillaries. That is one of the reasons—the thermal energy needed to affect wetting, that is the dissolution of the surface metal into the tin, is the other—why good reflow requires peak temperatures of Liquidus+20C. On voiding, I have yet to see any evidence of any problems for solder joints with the typical void contents observed. So my take is, do not worry too much about it; other things are much more important for reliability. Werner Engelmaier Engelmaier Associates, L.C. Electronic Packaging, Interconnection and Reliability Consulting 7 Jasmine Run Ormond Beach, FL 32174 USA Phone: 904-437-8747, Fax: 904-437-8737 E-mail: [log in to unmask], Website: www.engelmaier.com ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################